Super Wọ-sooro Nikan dabaru
  • Super Wọ-sooro Nikan dabaruSuper Wọ-sooro Nikan dabaru

Super Wọ-sooro Nikan dabaru

Iyatọ yiya resistance bẹrẹ pẹlu didara didara Super Wear-Resistant Single skru. A yan irin nitrided Ere (gẹgẹbi 38CrMoAlA) lati rii daju pe mojuto naa lagbara ati ti o tọ, pese ipilẹ to lagbara fun imudara oju.

Ọja paramita

Paramita

Awọn alaye

Dabaru Opin

Awọn alaye ti o wọpọ pẹlu 35mm, 45mm, 65mm, 75mm, 85mm, 90mm, bbl Fun apẹẹrẹ, nigbati o ba n ṣiṣẹ awọn paipu PVC, dabaru 65mm kan ni lilo pupọ bi o ṣe ṣaṣeyọri iwọntunwọnsi to dara laarin iṣelọpọ ati agbara agbara.

Gigun-si-Ipin Ipin (Ipin L/D)

Ni gbogbogbo awọn sakani lati 20:1 to 30:1. Fun awọn pilasitik ti o ni igbona bi PVC, ipin L/D nigbagbogbo wa laarin 20:1 ati 25:1. Eyi ṣe idaniloju pilasitik ti o to lakoko ti o dinku akoko ibugbe ti awọn ohun elo ninu agba lati dinku eewu jijẹ.

Rati funmorawon

Ni deede ṣubu laarin 3.5: 1 ati 4.5: 1. Iwọn funmorawon ti o tobi julọ n ṣe irọrun pilasitik ni kikun ati idapọ ti awọn ohun elo PVC.

Dabaru ikanni Ijinle

Ikanni dabaru jẹ aijinile jo, paapaa ni apakan wiwọn. Apẹrẹ yii dinku akoko ibugbe ti awọn ohun elo ati dinku iṣeeṣe ti ibajẹ.

Nọmba ti Alapapo ati Itutu agbegbe

Yatọ da lori iwọn ila opin ati awọn pato ohun elo, nigbagbogbo lati awọn agbegbe 5 si 6. Fun apẹẹrẹ, extruder kan-skru pẹlu iwọn ila opin 65mm le ni alapapo 6 ati awọn agbegbe itutu agbaiye lati jẹki iṣakoso iwọn otutu deede ni apakan kọọkan.

Iyara dabaru

Iwọn iyara nilo lati tunṣe ni ibamu si iwọn ila opin dabaru pato ati awọn ibeere iṣelọpọ. Fun φ65mm skru, nigbati o ba nmu awọn paipu pẹlu sisanra ogiri 3mm, iyara ti a ṣe iṣeduro ni iṣakoso laarin iwọn 25-35rpm.

Wakọ Agbara

Jẹmọ si dabaru iwọn ila opin ati ki o wu. Fun apẹẹrẹ, extruder kan-skru pẹlu iwọn ila opin 65mm kan ni igbagbogbo ni agbara awakọ ti 45-90kw.

Awọn iwọn otutu ti nṣiṣẹ

Iwọn otutu ti apakan ifunni jẹ gbogbo 160-170 ℃, apakan yo jẹ 180-190 ℃, ati apakan ori ku jẹ 175-185 ℃.

Ẹya Ọja Ati Ohun elo

1. Double-metal Super Wear-Resistant Single Screw , Lo irin agbara-giga bi ohun elo mimọ

2. Alloy Super wear-resistance agba, Awọn ihò inu ti sobusitireti erogba irin ti wa ni simẹnti centrifugalally tabi Layer ti alloy sooro, lile ti alloy kọja HRC 60.

3. Fun awọn ipo ti o ga julọ ti o ga julọ, a funni ni idaniloju ti igbesi aye ọja.

Super wear-sooro agba skru, o dara fun gilasi okun fikun pilasitik (GF), ti o ni awọn kalisiomu kaboneti, talc lulú, ga-išẹ atunlo ohun elo, tunlo egbin, ati awọn pilasitik ipata, ati be be lo.

4.O wulo si ọpọlọpọ awọn ohun elo, GFPA GFPBT GFPPS GFPP GFPOM CF PPS ...

Super Wear-Resistant Single ScrewSuper Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw

Awọn alaye iṣelọpọ

1. PTA ti wa ni lilo lati ṣe alurinmorin lori oke ati awọn ẹgbẹ ẹgbẹ ti awọn okun ti dabaru, eyi ti o jẹ awọn agbegbe prone lati wọ.

2. Ion nitriding àbábọrẹ ni a denser microstructure ati ki o ga líle (to HV1000-1200), pẹlu kere abuku.

3.The dada ti dabaru ti wa ni sprayed tabi ti a bo pẹlu tungsten carbide (WC), nickel-orisun alloys, etc.The iṣẹ aye le ti wa ni pọ nipa 3 to 8 igba.

Super Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw
Super Wear-Resistant Single ScrewSuper Wear-Resistant Single Screw
Fi ibeere ranṣẹ
Alaye olubasọrọ
  • Adirẹsi

    Àkọsílẹ C, No.2 Apa Iwọ-oorun, Xingzhou Avenue, Dinghai District, Zhoushan City, Zhejiang Province

Kaabo si oju opo wẹẹbu wa! Fun awọn ibeere nipa awọn ọja wa tabi atokọ idiyele, jọwọ fi imeeli rẹ silẹ si wa ati pe a yoo kan si laarin awọn wakati 24.
X
A nlo awọn kuki lati fun ọ ni iriri lilọ kiri ayelujara ti o dara julọ, ṣe itupalẹ ijabọ aaye ati ṣe iyasọtọ akoonu. Nipa lilo aaye yii, o gba si lilo awọn kuki wa. Asiri Afihan
KọGba