Awọn ọja
Non-Intermeshing Parallel Twin dabaru Barrel
  • Non-Intermeshing Parallel Twin dabaru BarrelNon-Intermeshing Parallel Twin dabaru Barrel

Non-Intermeshing Parallel Twin dabaru Barrel

Nanhaiya Non-Intermeshing Parallel Twin Screw Barrel ti jẹ apẹrẹ daradara fun PVC, PE, ati awọn laini extrusion WPC. Lati ibẹrẹ rẹ bi olupilẹṣẹ agba agba agba ọjọgbọn ni Ilu China ni ọdun 2014, Nanhaiya ti ṣe pataki ni igbagbogbo jiṣẹ awọn solusan extrusion oke-ogbontarigi ti kii ṣe idiyele ifigagbaga nikan ṣugbọn tun rii daju iṣẹ iduroṣinṣin. Nigbati awọn alabara pinnu lati ra Ti kii-Intermeshing Parallel Twin Screw Barrel lati Nanhaiya, wọn n ṣe idoko-owo ni ọja olokiki fun iwọntunwọnsi iyipo to dara julọ, ṣiṣe iṣelọpọ iyalẹnu, ati igbesi aye ṣiṣe ti o gbooro sii. Awọn abuda wọnyi jẹ ki o jẹ aṣayan lilọ-si fun awọn alabara kariaye ni ilepa ohun elo extrusion ti o gbẹkẹle ati iṣẹ ṣiṣe giga.

Nanhaiya Non-Intermeshing ni afiwe ibeji dabaru agba nṣiṣẹ ni afiwe sugbon ma ṣe intermesh, atehinwa rirẹ-rẹ nigba ti mimu dédé ohun elo gbigbe. Iṣeto ni idilọwọ ikojọpọ ooru ti o pọ ju ati ṣetọju awọn ohun-ini ohun elo. A ṣe agba naa lati inu irin alloy Ere, ti o ni ila pẹlu nickel-tungsten carbide, ati ẹrọ titọ lati rii daju awọn ifarada to muna. O dara fun iṣelọpọ polima, iṣelọpọ WPC, ati awọn ohun elo ti o nilo mimu iṣọra lakoko extrusion.

Apejuwe Ọja (Ipato)

Ohun elo

38CrMoAlA

Ooru Itoju Lile

HB260-320

Nitriding Lile

HV950-1000

Nitriding Ijinle

0.50-0.70mm

Nitriding Brittleness

Ipele 1

Irora

Ra0.4

Dabaru Titọ

0.015mm

Chrome Plating Lile

HV≥950HV

Sisanra Chrome

0.05-0.10mm

Bimetal Lile

HRC60-65

Ijinle Bimetal

2.0-3.0mm

Ẹya Ọja ati Ohun elo

Awọn agba ti kii ṣe intermeshing ni a lo nibiti rirẹ kekere ati dapọ pẹlẹbẹ nilo. Wọn jẹ apẹrẹ fun awọn profaili PVC, decking WPC, ati awọn thermoplastics ifura. Agba naa ngbanilaaye awọn ipin kikun ti o ga julọ lakoko mimu iduroṣinṣin ohun elo ati didara ọja ni ibamu.

Non-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw Barrel

Awọn alaye iṣelọpọ

Ọkọọkan Nanhaiya ti o jọra ibeji skru agba n gba ẹrọ CNC ti ilọsiwaju ati lilọ konge. Ilẹ ti pari-digi lati dinku edekoyede ati ilọsiwaju ṣiṣan ṣiṣu. Ofurufu dabaru jẹ lile nipasẹ nitriding tabi bimetallic alloy ti a bo fun iduroṣinṣin igba pipẹ.

Non-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw Barrel
Fi ibeere ranṣẹ
Alaye olubasọrọ
  • Adirẹsi

    Àkọsílẹ C, No.2 Apa Iwọ-oorun, Xingzhou Avenue, Dinghai District, Zhoushan City, Zhejiang Province

Kaabo si oju opo wẹẹbu wa! Fun awọn ibeere nipa awọn ọja wa tabi atokọ idiyele, jọwọ fi imeeli rẹ silẹ si wa ati pe a yoo kan si laarin awọn wakati 24.
X
A nlo awọn kuki lati fun ọ ni iriri lilọ kiri ayelujara ti o dara julọ, ṣe itupalẹ ijabọ aaye ati ṣe iyasọtọ akoonu. Nipa lilo aaye yii, o gba si lilo awọn kuki wa. Asiri Afihan
KọGba